ASTM F876 - PEX Tube - Dimensions

Dimensions of PEX tubes.

Dimensions of PEX SDR 9 (CTS) tube according ASTM F876 Standard Specification for Crosslinked Polyethylene (PEX) Tubing:

ASTM F876 - PEX Tube - Dimensions
Nominal Pipe Size
CTS
(inches)
Average Outside Diameter
(inches)
Min. Wall Thickness
(inches)
Average Inside Diameter
(inches)
1/2 0.625 0.070 0.510
3/4 0.875 0.097 0.681
1 1.125 0.125 0.875
1 1/4 1.375 0.153 1.069
1 1/2 1.625 0.181 1.263
2 2.125 0.236 1.653
2 2 1/2 2.625 0.292 2.041
3 3.125 0.347 2.431

Related Topics

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2018). ASTM F876 - PEX Tube - Dimensions. [online] Available at: https://www.engineeringtoolbox.com/ASTM-F876-PEX-tube-d_2139.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.16.12

.