Copper Tubes - Expansion Loop Capacity

Capacity of copper tubes expansion loops.

Expansion loop capacities of copper tubes type K are indicated in the chart below. 

Pipe expansion loop

Expansion loop capacity - copper pipe type k

Piping should be pre-stressed when anchored to minimize the stress in the system under normal operating conditions. 

Related Topics

  • Temperature Expansion

    Thermal expansion and expansion coefficients. Expansion pipes and tubes made of stainless steel, carbon steel, copper, plastics and more.

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2010). Copper Tubes - Expansion Loop Capacity. [online] Available at: https://www.engineeringtoolbox.com/copper-tubes-expansion-loops-d_1581.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.16.12

.