Concrete Slabs - Required Thickness

Required thickness of concrete slabs.

Concrete slab - thickness

  • Driveways : 6 - 8 inches ( 0.15 - 0.2 m)
  • Side walks, barn and granny floors : 5 - 6 inches (0.125 - 0.15 m)
  • Porches, Home garage floors : 4 - 5 inches (0.1 - 0.125 m)
  • Farm building floors, Home basement floors : 4 inches (0.1 m)

Related Topics

  • Miscellaneous

    Engineering related topics like Beaufort Wind Scale, CE-marking, drawing standards and more.

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2009). Concrete Slabs - Required Thickness. [online] Available at: https://www.engineeringtoolbox.com/thickness-concrete-slabs-d_1481.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.16.12

.